hello, could you do an api 598 or api 6d test connecting the valves in series in tandem

this would be allowed by the norm

Thank you
 
Replies continue below

Recommended for you

You should be able to do the body/shell tests this way.

However, you need to test each ball in each direction and you need to directly observe for any visible leakage, which I don't think is very practical in such a configuration.
 