Hi
Is Titanium Grade 12 (Ti-0.3Mo-0.8Ni) be used at -40C application. The material is used as a shell for a heat exchanger. During de-compression we may experience temperatures reaching -40C
Any help is appreciated. Thanks
Is Titanium Grade 12 (Ti-0.3Mo-0.8Ni) be used at -40C application. The material is used as a shell for a heat exchanger. During de-compression we may experience temperatures reaching -40C