Titanium valve vs inconel valve

Status
Not open for further replies.

schroon

Industrial
Mar 20, 2005
2
Why do engine builders use a titanium intake valve and a inconel exhaust valve in a blown gas motor? In a blown alcohol motor we use titanium intake and exhaust.
 
Replies continue below

Recommended for you

Heat resistance.

We use Titanium intake and Inconel exhaust in blown alcohol as we feel the exhaust valve can get to hot for Titanium at the HP levels we are getting.

Regards
pat pprimmer@acay.com.au
eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
In the alcohol motor I know we run 900-1000 pipe temperature at the end of the run. Does the gas motor run hotter? I only run about 12 pounds of boost with 9:1 compression whereas the alcohol is 12.8:1 with about 37-40 pounds of boost.
 