I have been looking for a source of proper torque for pipe threads on PVC Schedule 80 pipe. Most sources list a number of turns method (2 turns past finger tight, 1/2 turn past hand tight, etc.) This seems very open to me. Whose fingers and whose hands?
 
Replies continue below

Recommended for you

The Machinery's Handbook provideds a length in inches for 'handtight engagement'. (pg 1613, 23rd edition) Tommy
 