Hello,
The replica examination shows some cavities (acc. to focus changing) along grain boundaries. Electropolishing and Kalling's reagent was used in this case.
I have some doubts about cavities formation reason. What is your opinion? Thank you in advance!
The replica examination shows some cavities (acc. to focus changing) along grain boundaries. Electropolishing and Kalling's reagent was used in this case.
I have some doubts about cavities formation reason. What is your opinion? Thank you in advance!