Working on a battery with a steel casing.
Steel casing is lined with graphite paint but the zncl2 inside the battery still reacts with the steel.
Does Ag react with ZnCl2 ? is there a way to coat Pure graphite on steel (enough to prevent the reaction with ZnCl2)
I have tried to use 0.02mm pure graphite flake foil whoch seems to work but will be cost prohibitive in mass production.

Thanks
 
How do other similar chemistry batteries do it?

TTFN
faq731-376
7ofakss

Need help writing a question or understanding a reply? forum1529


Of course I can. I can do anything. I can do absolutely anything. I'm an expert!
There is a homework forum hosted by engineering.com:
 
Well , the idea is a new technology we are working on.
Other chemistry batteries do not have the issue of zncl2 , in our research we are bound by zncl2 for other reasons.
Graphite does protect the steel but trying apply it to the inside of a can is still a challenge.

 
ZnCl2 battery chemistry appears to have been around for a long time: It looks like there's supposed to be metallic zinc electrode that would protect an external steel casing?

TTFN
faq731-376
7ofakss

Need help writing a question or understanding a reply? forum1529


Of course I can. I can do anything. I can do absolutely anything. I'm an expert!
There is a homework forum hosted by engineering.com:
 
Again , I am looking to prevent the zncl2 reacting with steel by means of a conductive barrier coating , I think I have passed the basic battery chemistry lessons.
Zinc acts as an anode in a conventional zinc-carbon battery and does not use a steel can for conductivity.
I am looking for insight as to how best apply a pure graphite coating or alternative coating such as Ag to prevent short circuiting as a result of zncl2 reacting.
 
It would be best to electroplate Silver, I think. But, you may have to deal with oxidation of the silver. Have you thought about chrome/nickel steel:
TTFN
faq731-376
7ofakss

Need help writing a question or understanding a reply? forum1529


Of course I can. I can do anything. I can do absolutely anything. I'm an expert!
There is a homework forum hosted by engineering.com:
 
Thank you IRstuff , this is a big help.