Hello Everyone,
A newbie here.
Construction Code : ASME VIII Div 1
Qualification Code : ASME IX
Background :
A T-TS mock up PQR has been welded with a seal weld (one pass with filler), which is 3mm Fillet. Even though there is no Groove in its joint design, but it was having a counter sinking of 0.5mm R on the edges of tubesheet holes.
Question: Does the PQR get qualified in position for 5F only (considering its only fillet weld) or would it be having 5F+5G (considering there the edges to the root side of fillet is a bit machined for 0.5mm).?
looking forward to your quick help guys.
Thanks
A newbie here.
Construction Code : ASME VIII Div 1
Qualification Code : ASME IX
Background :
A T-TS mock up PQR has been welded with a seal weld (one pass with filler), which is 3mm Fillet. Even though there is no Groove in its joint design, but it was having a counter sinking of 0.5mm R on the edges of tubesheet holes.
Question: Does the PQR get qualified in position for 5F only (considering its only fillet weld) or would it be having 5F+5G (considering there the edges to the root side of fillet is a bit machined for 0.5mm).?
looking forward to your quick help guys.
Thanks