Is it allowed to have two welding operators (Machine TIG)to qualify on one weld coupon?
 
Replies continue below

Recommended for you

Yes. Refer to e.g. table QW-452.1(a), note (2).
 
See also QW 306 and QW 452.1 (b) Note 1
 