22350
Automotive
- Jul 2, 2010
- 4
I have a Velocette 250cc flat twin two stroke.
As nothing was available for the engine, we made the following modifications:
Wiseco Pistons
Nikasil steel cylinders
Modernized combustion chambers.
We just finished rebuilding it and started jetting.
The bike was very over-jetted and we brought it into line.
We are having a knocking problem. We have to severely over-jet the bike to get the knocking to go away. Like smoke screen over-jetting.
The original compression ratio was 7.5:1. Our current compression is 11:1
The knocking is heat related, but we don't see evidence of detonation on the plugs. Plug color is good, but rich.
We are running AMSOIL AT 32:1, which is less than the manufacturer's 20:1.
The bike does have smallish cooling fins:
<<
Here is the engine design notes:
<<
Any ideas?
Thanks,
Paul
As nothing was available for the engine, we made the following modifications:
Wiseco Pistons
Nikasil steel cylinders
Modernized combustion chambers.
We just finished rebuilding it and started jetting.
The bike was very over-jetted and we brought it into line.
We are having a knocking problem. We have to severely over-jet the bike to get the knocking to go away. Like smoke screen over-jetting.
The original compression ratio was 7.5:1. Our current compression is 11:1
The knocking is heat related, but we don't see evidence of detonation on the plugs. Plug color is good, but rich.
We are running AMSOIL AT 32:1, which is less than the manufacturer's 20:1.
The bike does have smallish cooling fins:
<<
Here is the engine design notes:
<<
Any ideas?
Thanks,
Paul