newweldeng09

Mechanical
Oct 31, 2008
84
I have feet that are to be welded to a pressure vessel. The feet are contructed of plate material and is to be welded to a forged pressure vessel. The weld symbol calls for a partial penetration single-bevel groove weld with a depth of 3/8" with a fillet reinforcement of 3/4". Is the governing thickness for determining impact requirements for the groove weld as stated in UCS-66(a)(1)(-a) or for fillet weld as stated in UCS-66(a)(1)(-b)?
 
Replies continue below

Recommended for you

newweldeng09, I can't imagine the feet are butt-welded to the vessel, so forget (-a), (-b) will govern. The MDMT for the joint is based on the thinner of the two parts joined. Impact test or exempt the joint members accordingly.

Now for the WELD METAL, see UCS-67.

Regards,

Mike
 
Thanks for the reply. Just for my own knowledge, if I had groove welds with fillet reinforcements, which par. would govern?
 
It is dependent on the joint configuration. If butt-welded, (a)(1)(a), corner joint (a)(1)(b). See also UCS-66(a), second paragraph, and (a)(1)(d). These concern the joint members only. Again, for weld procedures and weld metal, see UCS-67(a) and etc.

Regards,

Mike
 