Is interpretation VIII-1-89-308 valid?
Per UCS-66(a)(1)(b), 2 components welded to form corner joint, the thicker material exceeds 4 in, the thinner material is =<4", impact testing is required. This does not agree with the way UCS-66(a)(1)(b) is written?

 
Replies continue below

Recommended for you

Our AI lists that interpretation as "Caution - questionable". Pending further clarification, to be safe I would assume that it is invalid.
 