May 4, 2020 #1 edward995 Industrial May 4, 2020 9 why there is a line on the round bar? https://files.engineering.com/getfile.aspx?folder=ad0bb1c7-1caa-43e8-95da-9382c28f57a1&file=0fb37696-40e7-4fbc-be6f-24b8aecf9b16.jpg
May 5, 2020 #2 EdStainless Materials May 20, 2004 16,261 This looks to be hot finished bar. That line is from the hot rolling tooling. Have you tried to grind or turn a sample to see if it has depth? I doubt that it is a lapp or seam. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy Upvote 0 Downvote
This looks to be hot finished bar. That line is from the hot rolling tooling. Have you tried to grind or turn a sample to see if it has depth? I doubt that it is a lapp or seam. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy
May 5, 2020 #4 Guest Ditto. Not much to see here. "Everyone is entitled to their own opinions, but they are not entitled to their own facts." Upvote 0 Downvote
Ditto. Not much to see here. "Everyone is entitled to their own opinions, but they are not entitled to their own facts."