I am trying to determine what ASTM, UNS, or DIN, etc. number a certain metallurgical sample has, based on the following composition:
Al: .036
B: <.0005
C: .21
Cr: 1.3
Cu: .15
Mn: .48
Mo: .66
Nb: <.005
Ni: 1.71
P: .066
S: .013
Si: .26
Ti: <.005
V: .26
I have tried searching on several material sites with no success. Any guidance or tips would be greatly appreciated, thanks.
Al: .036
B: <.0005
C: .21
Cr: 1.3
Cu: .15
Mn: .48
Mo: .66
Nb: <.005
Ni: 1.71
P: .066
S: .013
Si: .26
Ti: <.005
V: .26
I have tried searching on several material sites with no success. Any guidance or tips would be greatly appreciated, thanks.