XL83NL
Mechanical
- Mar 3, 2011
- 3,109
Im reviewing a design for an 800H/HT vessel designed acc VIII-1. B16.9 straight tee's as per SB366 are required in 800H (WPNIC10) for the vessel. Theyre not listed in sect II-D. Pipe, flanges etc. are listed though, as is SB366 800 (WPNIC), hence are allowed to be used.
The vessels outlet pipe spool is designed acc. B31.3, and has the same size and main MoC (800H/HT). Appendix A of B31.3 lists B366 800H/HT tee's as per B16.9.
Could someone (maybe a commiittee member) point me the reason, if any, why section VIII-1 does not allow SB366 800H/HT fittings, e.g. tee's? I know there a several differences between VIII-1 and B31.3
The vessels outlet pipe spool is designed acc. B31.3, and has the same size and main MoC (800H/HT). Appendix A of B31.3 lists B366 800H/HT tee's as per B16.9.
Could someone (maybe a commiittee member) point me the reason, if any, why section VIII-1 does not allow SB366 800H/HT fittings, e.g. tee's? I know there a several differences between VIII-1 and B31.3