Im developing a spec where EN 1092-1 flanges (EN 10222-2 P245GH [1.0352]) have to be used in a B31.3 piping system.
Im using B31.3 304.7.2(a) to justify the use of EN 1092-1 flanges, as this standard is known for EN 13480 piping.
The flanges have a known and published rating, which covers part of it's p,T-rating. The wall thickness requirement also needs to be done to cover the 2nd part of the p,T-rating.
I check this using eq (3a) from 304.1.2. Since im dealing with a non-ASTM material spec, stress values have to be determined, which is done based on B31.3 302.3.2 (d).
Now here's the problem;
Where to find tensile strength values at temperature for P245GH flanges in EN 10222-2:2000? Table 2 only shows them for room temperature, whereas table 3 provides yield strength properties (Rp0,2) at temperature.
Any knows how to determine or get these?
Im using B31.3 304.7.2(a) to justify the use of EN 1092-1 flanges, as this standard is known for EN 13480 piping.
The flanges have a known and published rating, which covers part of it's p,T-rating. The wall thickness requirement also needs to be done to cover the 2nd part of the p,T-rating.
I check this using eq (3a) from 304.1.2. Since im dealing with a non-ASTM material spec, stress values have to be determined, which is done based on B31.3 302.3.2 (d).
Now here's the problem;
Where to find tensile strength values at temperature for P245GH flanges in EN 10222-2:2000? Table 2 only shows them for room temperature, whereas table 3 provides yield strength properties (Rp0,2) at temperature.
Any knows how to determine or get these?