Hi Experts,
Floating head heat exchanger.
Shell side medium: see water.
Shell side DP at DT: 26.3 bat at 150 deg.C
Shell side DP at DT: 17.2 bar at 70 deg.C
Shell ID: 450 mm
Floating falnge material: SB-283 C70620.
Client data sheet for the bolt material: UNS C70620.
Vendor uses the bolt material of SB-151 O 60 for the floating head flange. The bolt size will be 2.5" (63.5 mm). It is too large.
May anyone advise a higher permissible stress bolt material applicable to instead of SB-151 O 60.
Regards
Floating head heat exchanger.
Shell side medium: see water.
Shell side DP at DT: 26.3 bat at 150 deg.C
Shell side DP at DT: 17.2 bar at 70 deg.C
Shell ID: 450 mm
Floating falnge material: SB-283 C70620.
Client data sheet for the bolt material: UNS C70620.
Vendor uses the bolt material of SB-151 O 60 for the floating head flange. The bolt size will be 2.5" (63.5 mm). It is too large.
May anyone advise a higher permissible stress bolt material applicable to instead of SB-151 O 60.
Regards