Does anyone know what thermoplastics I should consider to weld onto fabrics using a hand held ultra sound welder at 20khz-40khz low amplitude?

I've heard two different answers for polyuretahne film adn am unsure about this material.

Thank you in advance.
 
Replies continue below

Recommended for you

Ultrasonic welding of plastics never worked worth a crap for me.

Okay, maybe I was holding my tongue wrong, but I did _everything_ the ultrasonic vendors said to do, and it still didn't meet my expectations.

If you haven't actually paid for the welder yet, consider buying a turnkey system, with a money- back guarantee.



Mike Halloran
Pembroke Pines, FL, USA
 