hello everyone,
I am modeling the axisymmetric tube hydroforming of aluminium tube by implicit analysis, the pressure is varied upto 22 MPa
For higher pressure from 15 MPa onwards I get the warning messages
The strain increment has exceeded fifty times the strain to cause first yield at 1331 points
The plasticity/creep/connector friction algorithm did not converge at 877 points
Convergence judged unlikely. Increment will be attempted again with a time increment of 2.25508e-03
FORCE equilibrium accepted using the alternate tolerance.
I have tried using a fixed time increment of 0.0001 but job is aborted
Is there any problem in material properties or in the step?
Thank you in advance
I am modeling the axisymmetric tube hydroforming of aluminium tube by implicit analysis, the pressure is varied upto 22 MPa
For higher pressure from 15 MPa onwards I get the warning messages
The strain increment has exceeded fifty times the strain to cause first yield at 1331 points
The plasticity/creep/connector friction algorithm did not converge at 877 points
Convergence judged unlikely. Increment will be attempted again with a time increment of 2.25508e-03
FORCE equilibrium accepted using the alternate tolerance.
I have tried using a fixed time increment of 0.0001 but job is aborted
Is there any problem in material properties or in the step?
Thank you in advance