Frank Burns
Industrial
- Nov 7, 2022
- 8
All,
I have been tasked with meeting a specification for hydrotest water purity that seems a little "stringent". Usually DI water was sufficient at other sites, however, now I have a new specification to meet with water purity as follows:
Chlorides 50 ppm max (SS) 100 ppm max (CS)
pH 6.5-9
Sulfate 42 ppm
Fatty Acids 14 ppm
Ammonium 3 ppm (max)
Bacteria(SRB ,APB ,etc.) insignificant or "very low" activity
Total Suspended Solids 30 ppm
Turbidity <1 Nephelometric Turbidity Unit
Total Organic Compound 4 ppm
Temperature < 120°F
I have exhausted my resources trying to find a lab that can test for "all" of the list and can't seem to find a vendor who can deliver water "pre-tested" and certified to meet all of the requirements above. I am reaching out to anyone with water purity experience for advice, vendors, etc. that can aid in what I am trying to meet. (Keep in mind, I am a mechanical guy and not a chemist), so any comments are welcome.
I have been tasked with meeting a specification for hydrotest water purity that seems a little "stringent". Usually DI water was sufficient at other sites, however, now I have a new specification to meet with water purity as follows:
Chlorides 50 ppm max (SS) 100 ppm max (CS)
pH 6.5-9
Sulfate 42 ppm
Fatty Acids 14 ppm
Ammonium 3 ppm (max)
Bacteria(SRB ,APB ,etc.) insignificant or "very low" activity
Total Suspended Solids 30 ppm
Turbidity <1 Nephelometric Turbidity Unit
Total Organic Compound 4 ppm
Temperature < 120°F
I have exhausted my resources trying to find a lab that can test for "all" of the list and can't seem to find a vendor who can deliver water "pre-tested" and certified to meet all of the requirements above. I am reaching out to anyone with water purity experience for advice, vendors, etc. that can aid in what I am trying to meet. (Keep in mind, I am a mechanical guy and not a chemist), so any comments are welcome.