timsch
Mechanical
- Oct 27, 2009
- 193
I have a 40" blind flange, 3" thick that will have a 5.5" diameter hole bored offcenter, with a 4" studded flange welded over that hole with a 3/4" inner fillet and a 9/16" outer fillet securing the studded flange. Design conditions are 150psi internal pressure & 320F, all materials 316L.
I have been tasked with performing weld calculations. I am referring to UG-37,-40,-41 & UW-15,-16 and following L-7.4 as the closest example I could find.
I was able to find some information on a studded flange for this calculation in Fig. UG-40(a-1), but I am uncertain about certain values to use for calculations, specifically values for A_2 shown in Fig. UG-37.1.
Per UG-40(a-1), t_n=0. For A_2 = 5*(t_n-t_rn)*f_r2*t, I will wind up with a negative number if I have any value for t_rn. If I just consider the cross sectional area of the studded flange itself, based on the hatched section of Fig UG-37.1, I come up with around 50 in^2, but this is not how the area is calculated per formulas for A_2.
What am I missing?
Thanks,
Tim
EDIT: To answer my own question, I am (was) missing UG-37(b)(2), and I've been barking up the wrong tree. UG-39 does not mention weld reinforcement. I just need to find the section in the code that covers weld calculations for my application
I have been tasked with performing weld calculations. I am referring to UG-37,-40,-41 & UW-15,-16 and following L-7.4 as the closest example I could find.
I was able to find some information on a studded flange for this calculation in Fig. UG-40(a-1), but I am uncertain about certain values to use for calculations, specifically values for A_2 shown in Fig. UG-37.1.
Per UG-40(a-1), t_n=0. For A_2 = 5*(t_n-t_rn)*f_r2*t, I will wind up with a negative number if I have any value for t_rn. If I just consider the cross sectional area of the studded flange itself, based on the hatched section of Fig UG-37.1, I come up with around 50 in^2, but this is not how the area is calculated per formulas for A_2.
What am I missing?
Thanks,
Tim
EDIT: To answer my own question, I am (was) missing UG-37(b)(2), and I've been barking up the wrong tree. UG-39 does not mention weld reinforcement. I just need to find the section in the code that covers weld calculations for my application