A consulting engineer has specified 3/4" DIA headed studs welded at a 45 DEG angle to a flat plate. I have searched and called around to our stud suppliers and they do not seem to have studs and ferrules available for this application. They suggest welding straight and then bending over. The other alternative is to grind standard studs at 45 DEG to get a decent fitup and then fillet weld. Obviously production would like to be able shoot these rather than fillet weld each one individually. Any thoughts or recommendations?