meltedEng
Mechanical
- Aug 24, 2017
- 47
Fellows,
We are going to be welding some Hastelloy G-35 to make a ASME vessel. We work with C276, C22, B2/3 occasionally, no issues. Obviously this is another class of the alloy group, and quite niche.
Any concerns different from C276? Any recommended reading? Anyone in here have experience with it?
Thanks
We are going to be welding some Hastelloy G-35 to make a ASME vessel. We work with C276, C22, B2/3 occasionally, no issues. Obviously this is another class of the alloy group, and quite niche.
Any concerns different from C276? Any recommended reading? Anyone in here have experience with it?
Thanks