Welding 304L to 321 SS
I had figured on using 347 welding rod to tig weld a tube spigot made of 304L to a 321 exhaust pipe. The tube is a condensate /rainwater drain.
A colleague of mine said Inco 82 would do a better job because of the higher nickel content.
I figure this is a situation where a little knowledge is dangerous. What are the pros and cons of using an inconel rod here?