Hello,
I've never used Pipes with A53 Gr.B Steel for structural purposes, only A500, but a cliente has a supplier who sells these Pipes and he wants to use It.
I saw that the AISC Spec. considers A53 Gr.B as one of the HSS approved steels. My question is if there are some restrictions to welding of this material. Since it's a steel more appropriate for fluid conduction, i'm not well aware and am afraid to specify some inadequate weld process.
Thanks in advance.
I've never used Pipes with A53 Gr.B Steel for structural purposes, only A500, but a cliente has a supplier who sells these Pipes and he wants to use It.
I saw that the AISC Spec. considers A53 Gr.B as one of the HSS approved steels. My question is if there are some restrictions to welding of this material. Since it's a steel more appropriate for fluid conduction, i'm not well aware and am afraid to specify some inadequate weld process.