We're trying to autogenously weld 465 with itself. Just wondering if anyone has seen this at all or given it a try.
We have had success with welding 465 to 17-4 ( can get some ferrite from the 17-4), but can't seem to get 465 to weld without severe cracking. I'm prone to think this will be very difficult but wanted to see if anyone has any input