Guys, please offer your suggestion.
Base metal in PQR: P1-Group 1 TO P1-Group 2
Base metal in WPS: P1-Group 2 TO P1-Group 2
Welding process: SMAW
Impact test is required.
Can I use the above mentionen PQR to support this WPS, if I use ASME IX?
For my understanding, in ASME IX, PQR base metal should have the same P number and Group Number as the WPS base metal, if impact test required.
Please advice. thanks.