Dear Mr./Mrs./Miss.
The air cooler in HYDROCRACKER unit (oil refining plant)have the below specifications,Please guide me about the welding procedure ,filler metal and any requirements in conform to service.
design pressure:55.3 bar/f.v
design temperature:171 celsius
fluid circulated: H2+HCBN TRACES
X-ray examination:spot
PWHT:yes (Max. weld hardness;200 brinnel)
Materials:SA-516Gr.60 , SA-105 , SA-234WPB
Headers Thk.:30 mm.
With best regards.
GRH
23 Feb. 2011
The air cooler in HYDROCRACKER unit (oil refining plant)have the below specifications,Please guide me about the welding procedure ,filler metal and any requirements in conform to service.
design pressure:55.3 bar/f.v
design temperature:171 celsius
fluid circulated: H2+HCBN TRACES
X-ray examination:spot
PWHT:yes (Max. weld hardness;200 brinnel)
Materials:SA-516Gr.60 , SA-105 , SA-234WPB
Headers Thk.:30 mm.
With best regards.
GRH