Dear All,
I have my ferromagnetic type stainless steel 4031 grade machined to the desired shape. since there was a slut with 1600(length)*80(width)*10(depth)mm dimension on the plate wich the machining operator was going to machine it to the mentioned dimensions.
but he has mistaken and machine 2mm extra in depth. and now I have a slut with 1600*80*12.
now I am figuring out to recover the depth of slut using some method like welding or metal spraying and then machine it to the desired depth.
wich welding method and welding rod(electrode) are suitable for the 4031 stainless steel? will it be economical to do so?
since the magnetic properties of the plate is a concern(according to design intent, plate is going to operate in a magnetic solenoid) will welding have an effect on the magnetic properties of the plate?
any comment would really be aprecieted.
I have my ferromagnetic type stainless steel 4031 grade machined to the desired shape. since there was a slut with 1600(length)*80(width)*10(depth)mm dimension on the plate wich the machining operator was going to machine it to the mentioned dimensions.
but he has mistaken and machine 2mm extra in depth. and now I have a slut with 1600*80*12.
now I am figuring out to recover the depth of slut using some method like welding or metal spraying and then machine it to the desired depth.
wich welding method and welding rod(electrode) are suitable for the 4031 stainless steel? will it be economical to do so?
since the magnetic properties of the plate is a concern(according to design intent, plate is going to operate in a magnetic solenoid) will welding have an effect on the magnetic properties of the plate?
any comment would really be aprecieted.