I am working on a project with following water:

Sodium (Na+) mg/l 25,000.0
Carbonate (CO32-) mg/l 12000.0
Sulphate (SO42-) mg/l 1000.0
Chloride (Cl-) mg/l 22000.0
Total Dissolved Solids 70000.0
TSS mg/l 1800.0
pH 12-13
Silica (SiO2) mg/l 5000.0
Insoluble oil (oil & grease) mg/l 100 - 150
Total Organic Carbon: normal mg/l 4000.0
Temperature ºC 90 - 100

Any body have idea what kind of material or lining will have resistance to this water?