Why the distorsion is caused in multilayer curved glasses? 1

Status
Not open for further replies.
Replies continue below

Recommended for you

Refractive index differences between the layers. Light ray path length differences through the various refractive indices. "Lens" effect of light rays bending differently depending upon the angle of incidence with respect to the curved surface. Any introductory book on optics or light physics will explain the concepts in greater detail.

Bruce
 
An excellent source of such information is Konrady's "Applied Optics and Optical Design" This is an old classic that has been reprinted by Dover publications and it is very clear and understandable and covers your topic very well.

 