XM-19 (UNS20910 HS) Round Bar

Status
Not open for further replies.

rajnad

Materials
Nov 7, 2011
7
Hi Friends,

I have a query. Is it possible to have the below properties in a Xm-19 Bar ?

YS ≥ 850 Mpa
TS ≥ 1000 Mpa
Kv ≥ 45 (196°C)

In case the bar is strain hardened, the required Kv properties would not be achievable ?

Thanks
 
Replies continue below

Recommended for you

You should contact your vendor for this material and ask them these questions directly.
 
Looks reasonable depending on size and any other potential requirements. You can reach out to Carpenter Technology.
 
I have only seen those properties up to about 1.5" diameter.
You know that you could buy some pieces off the shelf to test?
Aqumet.com
This ia used as boat prop shafting and you could buy short pieces.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 