JourneymanEng
Mechanical
I am trying to conduct a simple FEA on a Stainless component that will experience temperatures in excess of 650 degrees C.
Problem:
I would like to change the material properties of the Steel i am using to establish the maximum deflection under load.
While my FEA package (ALGOR) will allow for temperature input, i find that achieving a uniform temperature in the model creates a large unworkable mesh.
I am innexperienced with Algor, but have used material property changes with other packages to good effect.
Is there a reference for changes in E or G for Stainless 316/321/304? The usual sources reveal nowt.
Peter
Problem:
I would like to change the material properties of the Steel i am using to establish the maximum deflection under load.
While my FEA package (ALGOR) will allow for temperature input, i find that achieving a uniform temperature in the model creates a large unworkable mesh.
I am innexperienced with Algor, but have used material property changes with other packages to good effect.
Is there a reference for changes in E or G for Stainless 316/321/304? The usual sources reveal nowt.
Peter