Apr 14, 2022 #1 Abu Ali Materials Jul 24, 2014 5 0 0 AE Hi how to calculate or find A269 tubes 316L tube hydrotest pressure for all size when you have OD and WT. thanks
Hi how to calculate or find A269 tubes 316L tube hydrotest pressure for all size when you have OD and WT. thanks
Apr 14, 2022 #2 XL83NL Mechanical Mar 3, 2011 3,043 0 36 NL Design code determines the hydrotest. Or do you mean the test pressure required by ASTM A269? Huub - You never get what you expect, you only get what you inspect. Upvote 0 Downvote
Design code determines the hydrotest. Or do you mean the test pressure required by ASTM A269? Huub - You never get what you expect, you only get what you inspect.
Apr 14, 2022 #3 EdStainless Materials May 20, 2004 15,893 0 36 US If you mean just the tubes look in A1016, they didn't want to repeat this information in 14 different specs. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed Upvote 0 Downvote
If you mean just the tubes look in A1016, they didn't want to repeat this information in 14 different specs. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed
Apr 15, 2022 Thread starter #4 Abu Ali Materials Jul 24, 2014 5 0 0 AE @XL83NL thanks for your reply, yes I do mean the pressure Upvote 0 Downvote
Apr 15, 2022 Thread starter #5 Abu Ali Materials Jul 24, 2014 5 0 0 AE @EdStainless thanks I will look in to that Upvote 0 Downvote