HI,
after inject the mold , the parts has not air trap But outside the mold during get cooling , the air trap will apear ,the picture is attached.
part weight=170gr
thickness=20 mm
height=100 mm
width= 70mm
after inject the mold , the parts has not air trap But outside the mold during get cooling , the air trap will apear ,the picture is attached.
part weight=170gr
thickness=20 mm
height=100 mm
width= 70mm