kripton
Materials
- Aug 9, 2016
- 12
Hello there,
I have a PQR prepared/tested as per the API 1104 & B31.8 design code.
Is it possible to write a new WPS as per ASME IX & B31.3 using the same PQR.
PQR Included:
2xTensile Test as per API 1104
2xFace,2xRoot Bends as per API 1104
6 set (3) Charpy per ASTM E23-12c (HAZ & WCL)
2 set Hardness (V) per ASTM E384
Thx.
I have a PQR prepared/tested as per the API 1104 & B31.8 design code.
Is it possible to write a new WPS as per ASME IX & B31.3 using the same PQR.
PQR Included:
2xTensile Test as per API 1104
2xFace,2xRoot Bends as per API 1104
6 set (3) Charpy per ASTM E23-12c (HAZ & WCL)
2 set Hardness (V) per ASTM E384
Thx.