API 5L Grade X65MS (MS stands for) 2

Status
Not open for further replies.

goodbadgood

Materials
Sep 24, 2014
40
Hi

can anyone explain what does MS stands for in API 5L grade X65 MS Pipes?

thanks
 
Replies continue below

Recommended for you

Mild Steel?

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
Steve,
Just out of interest, where did you find that info ?
I only have an old edition of API 5L (2000) and all I could find was S was for seamless.
Cheers,
Shane
 
I didn't have my handy copy of 5L to hand earlier, but fully agree with S Jones (I knew he would be right).

Comes from the latest two versions of 5L - 44th and 45th edition when they amalgamated with ISO 3183.
M stands for thermomechanically rolled or formed to give it is full terminology.
S for sour service where it meets requirements of annex H.

So it does depend on whether this is relatively new pipe or the OP is talking about pipe to a different version of 5L - makes a big difference.....




Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 