ASME B16.5 Para. 6.3.2 says a raised face may be removed from a raised face flange to convert it to a flat face flange, provided that the required dimension, tf, shown in Fig. 6 (Fig. II-6 of Mandatory Appendix II) is maintained.
ASME PCC-2 Para. 3.1 says under-thickness of a raised face due to refinishing shall be acceptable, provided the minimum finished height of the raised face is 0.8 mm (0.031 in.).

I would appreciate it if somebody could explain to me why PCC-2 wants to keep 0.031" of the raised face when B16.5 allows to complete removal. Is that for serration of the face?
 
Replies continue below

Recommended for you

B16.5 allows removal of raised face when converting to a flat faced flange. PCC-2 requires maintaining 0.8mm of raised face when refinishing, i.e. still using the flange as a raised face flange. This is to minimize the risk of the flange contacting the centering ring and rotating of the gasket sealing element.
 