Hi all,

I have to estimate the argon gas consumption for a pressure vessel of ss304L having a dia of 1m and height 1.98m. Total weld length will be almost 9 m (6mm Thick) What will be the argon gas consumption during the welding.? (Cylinder Wise) (Excluding purging)

Please help
 
Replies continue below

Recommended for you

how long will you be welding?
argon flow is measured in cu f/h or litres/minute, value should be around 15-20 cf/h or 7-10 l/min (I'm thinking TIG or GTAW here).

time x argon flow = total volume of Ar consumed.
 
THANK YOU KINGNERO FOR THE ANSWER. THAT HELPED A LOT.
 