planc
Structural
- Mar 3, 2022
- 64
We removed the bituminous membrane sheet and the topping above the membrane because of some leaks. You can still see the old membrane on the upper sides at the edges not yet teared or pulled up. (and the lower left side whose topping were not chipped).
but you can see, the membrane has no separate drain on each own. It drain is taken by the concrete topping above. But ever years when the topping cracks or the membrane cracks. Its difficult to tell them from each other.