USAeng
Mechanical
- Jun 6, 2010
- 419
We have fans that send biogas to a flare. We had a neoprene seal that is basically a hole cut in neoprene with the motor shaft stuck through then the impeller was direct drive mounted to the motor. That leaked too much gas so the OEM switched to a Teflon plate with a hole machined that the shaft fit through with a tight tolerance- still direct drive - still leaked. Now we are looking at a coupled design which gives them more room to put in a double lip seal around the shaft.
I believe this will work but wonder if anyone has an experience to share? We also looked at a John Crane seal but they were very expensive.
We are running the blowers at 3450RPM but only for about 5-10 minute intervals normally about 8 times daily. If the plant is down then they will flare for longer periods but that will be abnormal.
Thanks for any advice
I believe this will work but wonder if anyone has an experience to share? We also looked at a John Crane seal but they were very expensive.
We are running the blowers at 3450RPM but only for about 5-10 minute intervals normally about 8 times daily. If the plant is down then they will flare for longer periods but that will be abnormal.