We got asked to weld using ER16-8-2 for 310 SS for vessel work.
We have a standard P8 to P8 procedure. The procedure has the standard AWS D1.6 table showing basic rods under P8 we can use for different recommended base materials. The QA said he believes we cannot use this procedure for ER16-8-2 for 310 base materials. But the material is P8, the rod classification is non-essential, so we are not sure why the QA has rejected this?
We have a standard P8 to P8 procedure. The procedure has the standard AWS D1.6 table showing basic rods under P8 we can use for different recommended base materials. The QA said he believes we cannot use this procedure for ER16-8-2 for 310 base materials. But the material is P8, the rod classification is non-essential, so we are not sure why the QA has rejected this?