Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Ferric Sulphate feed line problems

Status
Not open for further replies.

5wp

Civil/Environmental
Joined
Nov 6, 2006
Messages
51
Location
CA
We feed ferric sulphate thru a 1" pvc line to our water plant clarifiers. I've noticed that the line will get partially plugged after 3 or 4 years, to the point that the line is only half available .
We store the ferric sulphate in fibrglass tanks.
Could the precipitated out material in the pipe be coming from the tank?
If not then why does the line build up like this?
Does ferric sulphate normall precipitate out in the lines forming a
rather hard material? The ferric sulphate is fed neat.
Any suggestions??
 
Many users will dilute the water treatment chemicals to 5% solution strength to avoid the problem that you describe.
 
bimr
Thanks. We'll give it a try.
 
We have the same problem on occassions. As a routine we flush our dosing lines every 6 months to remove any build-up.
 