Can we weld two tubes together to meet the total length requirement? We have fire tube boiler operates at 12 bar pressure. The available tubes are short in length by a meter, therefore we intend to join two tubes together in a way to fit to the required size. If it is allowed by the code, what considerations one should keep in mind?
 
See ASME 1 2023 Table PW-11

Regards
 
You can buttweld up to 9 short pieces of tube together to make one tube

If anyone asks for your justificatin, say that "someone on the internet told you it was acceptable ;)

Regrds

MJCronin
Sr. Process Engineer
 
Dammit, I was hoping to use 10 :)

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
Sorry, ... the rules are the rules ...

MJCronin
Sr. Process Engineer
 
I'm not familiar enough with Section I to answer the question, but my guess is that this is likely allowed. Check with your A.I.

There is a false perception that anything that looks like a poor design practice is expressly prohibited by ASME Code, but the reality is that many things that would be considered a poor practice (e.g. nozzles located directly on weld seams, nozzles located in the knuckle region of a head, nozzle attached with partial penetration welds, vessels fabricated out of more individual plates than is absolutely necessary, repads overlapping weld seams, square/rectangular repads with sharp corners, repads thicker than the vessel wall thickness, etc.) are perfectly acceptable per ASME Section VIII.


-Christine
 
During the manufacture of a heat exchanger I did not approve a shell made up of 2 sections of NPS 12 to complete the total length of 2000 mm.
I was not a serious manufacturer.

Regards
 
During manufacturing some errors can occur that require user approval to continue with the work. But I never saw a nozzle on a longitudinal/circumferential weld on the design drawing, for example.

Regards
 
Follow 3.3.4.9 part.3 of NBIC, repair of firetube boiler.
 