Hello!
I am designing a product that is inserted into potable water applications. I am looking for a high strength (~16 ksi yield strength, 1000 ksi elastic modulus) plastic that is NSF-61 certified.
I have tried Delrin 150 NC010 (10 ksi yield strength, 420 ksi elastic modulus), but it ended up being too weak and flexible. I found Zytel 77G33L NC010 (25 ksi yield strength, 1200 ksi elastic modulus) today, which looks like it might work well, but I am hoping to find a few other options.
Ideally, the plastic would be readily available in stock materials, and then able to be molded, extruded, or machined to final form. Water absorption is also a factor; the less, the better (Zytel is .30% after 24 hours).
Thank you for the help!
I am designing a product that is inserted into potable water applications. I am looking for a high strength (~16 ksi yield strength, 1000 ksi elastic modulus) plastic that is NSF-61 certified.
I have tried Delrin 150 NC010 (10 ksi yield strength, 420 ksi elastic modulus), but it ended up being too weak and flexible. I found Zytel 77G33L NC010 (25 ksi yield strength, 1200 ksi elastic modulus) today, which looks like it might work well, but I am hoping to find a few other options.
Ideally, the plastic would be readily available in stock materials, and then able to be molded, extruded, or machined to final form. Water absorption is also a factor; the less, the better (Zytel is .30% after 24 hours).
Thank you for the help!