EngDM
Structural
- Aug 10, 2021
- 744
Is it possible to use 2x6 oriented horizontally as your shearwall sheathing? There are tables in O86 for diagonal member paneling, but I couldn't find anything for horizontal. My gut is saying no, because there is no shear transfer between adjacent horizontal members. With diagonal members, at least the member can go into tension/compression and drag the base shear from the top chord to the bottom chord.
So aside from some sort of shear transfer detail between adjacent 2x6 panels I don't think this works.
Just looking for a sanity check or some insight.
So aside from some sort of shear transfer detail between adjacent 2x6 panels I don't think this works.
Just looking for a sanity check or some insight.