Is there a 'best' or most economical weld for a cap or end plate connection to an HSS member?
Assuming the cap plate will take load similar to this lifting lug problem:
You could weld around the inside or outside using a groove weld or you could oversize the plate and provide a fillet weld. Is there one in particular that is better or ones that should be avoided?
I would preferably use the outside complete-joint penetration square (or V) groove weld with backing. Any issues with that?
Thanks
EIT