Good day:

When the NDT tests have been carried out at 100% of the welded joints, the hydrostatic tests must be carried out or they may not be carried out in b31.3.

We have made a line of 3 km of tailings of 34 ".

Thanks for your help


Juan Torres
 
Replies continue below

Recommended for you

A hydrostatic test or a leak test is mandatory as per 345.1 to ensure tightness of the piping system.
Prior to initial operation, and after completion of the
applicable examinations required by para. 341, [highlight #FCE94F]each piping
system shall be tested to ensure tightness[/highlight]
 
Juan,
If your design is B31.3 you must follow the requirements - hydrotest required.
Without more information I would question why B31.3 is being used for 3km of above ground tailings ?
Regards,
Shane
 
It may be depended on the service fluid category and what are types of NDT tests have been performed, and if this is a "golden weld" as defined and acceptable by the Client.
 