Hey folks, need your opinion again. Part of my 1950 vessel has a 750oF design temp. I am installing SA516-70 & SA105 mat'l in this section. The 1950 ASME Code doesn't req. impact test or hardness limits. The 2004 Code, under UG-20(f) does. I believe it's due to the "creep-rupture range of C.S. at about 700oF" mentioned in API 510. We are allowed to design to the 1950 Code and NOT require impact test. I am recommending normalized, impact tested and limiting the hardness to 200BHN for adding our material to this section. One of the openings being added is a new 60"OD inlet and is a significant part of this section. Do you think I am being to Code critical by recommending these special material conditions, based on today's Code rather than the 1950 Code? I feel, better safe than sorry, especially since the added small cost of these test and conditions is not an issue.