lslcpfcc
Mechanical
- Jul 20, 2016
- 36
Dear
this is a problems on the RT films of piping welds, which one can give me a reasonable explanation.
on the films one indication (a dark line on the root weld edge ares )looks like lack fusion ,but as my and my friend many year experience, this is not the lack fusion.
the welding process is GTAW +SMAW for 6” pipeline
anyone can explain why this dark line appeared ?
this is a problems on the RT films of piping welds, which one can give me a reasonable explanation.
on the films one indication (a dark line on the root weld edge ares )looks like lack fusion ,but as my and my friend many year experience, this is not the lack fusion.
the welding process is GTAW +SMAW for 6” pipeline
anyone can explain why this dark line appeared ?