There's no reason why you couldn't, as long as the tank was designed and built to handle both the temperature and weight. Note that the temperature is low enough the manufacturer will need to use typical steels used in the manufacture of any cryogenic tank, but the density is considerably lower. Verify with the manufacturer that the tank can handle the weight.Hello Folks, I wonder if somebody has ever made the cool down of an LNG tank using liquid nitrogen.